Abstract

We present a systematic study of membrane structure (pore diameter and arrangement) in anodized aluminum oxide (AAO) layers obtained by anodization voltages 8-20 V in sulfuric and 15-40 V in oxalic acid electrolyte solutions. Anodization of bulk aluminum in sulfuric acid at 10 V potential was found to be optimal for production or ultrathin freestanding membranes with pore diameter in sub-20 nm range. The developed process with slow electrochemical reaction results in AAO membranes with thickness below 70 nm. The minimum required time for formation of continuous AAO membrane was determined and influence of electrolyte concentration on pore diameter in membrane after barrier layer removal analyzed. Finally, we demonstrate a method of membrane transfer onto a different surface and using it for masked deposition of dense nanoparticle arrays with diameters below 20 nm.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.