Abstract
This paper presents new findings on ultrasonic spray pyrolysis of zirconium hydroxyl acetate precursor drops whose sizes were precisely measured using laser light diffraction technique. Precursor concentration plays a predominant role in determination of product particle size. At 0.01 wt% precursor concentration, conventional spray pyrolysis at 750°C using precursor drops 5–8 μm in diameter, generated by an ultrasonic nebulizer at 2.66 MHz, yielded uniform spherical yttria‐stabilized zirconia (YSZ) particles 73 nm in diameter measured by scanning electron microscopy. The YSZ particle diameters were much smaller than those predicted by the one‐particle‐per‐drop mechanism. Under similar reaction conditions, the high‐throughput ultrasound‐modulated two‐fluid (UMTF) spray pyrolysis of larger precursor drops (28‐μm peak diameter) also yielded spherical dense particles; they were significantly smaller in size than those produced by the low‐throughput conventional ultrasonic spray pyrolysis of smaller drops (6.8‐μm peak diameter).
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.