Abstract

The purpose of this study was to examine weldability of an AA7072-cladded high-strength AA7075-T6 via ultrasonic spot welding, focusing on the influence of welding energy on mechanical properties and failure mechanisms. Defect-free sound joints were achieved with robust bonding and grain refinement via dynamic recrystallization at the weld interface, leading to superior static and fatigue properties. The nominal tensile lap shear strength increased with increasing welding energy, and exceeded AWS D17.2 standards at higher energy levels. Interfacial failure at higher cyclic loads with distinctive elongated shear dimples and fatigue striations and transverse through-thickness failure at lower cyclic loads were observed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.