Abstract
Ultrasonic and rotating bending fatigue tests were carried out for aged and nitrided Ni-base super alloys to investigate the effects of loading frequency and nitriding on fatigue strength. Loading frequencies were 19.5 kHz under ultrasonic and 50 Hz under rotating bending, respectively. Fatigue strength under ultrasonic was higher than that under rotating bending in both alloys. Moreover, in both tests, fatigue strength was improved by nitriding. The increase in fatigue strength by nitriding was large in ultrasonic fatigue. These results were discussed through the successive observation of fatigue process at specimen surface and fracture surface observation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.