Abstract

Aliphatic poly(H-phosphonate)s were obtained by polyesterification of dimethyl H-phosphonate with bio-based long-chain diols. Nonadecane-1,19-diol, tricosane-1,23-diol, and octatetracontane-1,48-diol with dimethyl H-phosphonate yield the corresponding polyphosphoesters (PPE19H, PPE23H, and PPE48H) with molecular weights (Mn) up to 4.3 × 104 g mol–1. Postfunctionalization of these polymers via Hirao cross-coupling yields the selectively functionalized poly(H-phosphonate)s PPE19Ph, PPE23Ph, and PPE48Ph. DSC analysis revealed significantly enhanced crystallinities and melting points (up to Tm = 110 °C) with increasing methylene sequence lengths. Hydrolytic degradation of polymer powder of poly-(H-phosphonate) occurred up to 95% in 2 days. The degradation rates decreased with increasing methylene sequence length. After postfunctionalization, degradation occurred only to a minimal extent over 3 months in basic and in acidic media.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.