Abstract

AbstractSpatial resolution of scintillator is crucial for high‐quality X‐ray imaging, especially in tiny and complicated electronic component. In this work, PrPP2MnBr4 single crystal is obtained by dual‐solvent evaporation method, which gives an unprecedented high spatial resolution of 104.3 lp/mm, representingstate of the art among non‐lead metal halides. The study also conducts the preparation of large area scintillation screen (10 cm × 10 cm) by solidifying melted salt PrPP2MnBr4, thus giving an excellent X‐ray imaging with spatial resolution of 53.5 lp mm−1, which demonstrates its application on large area detection.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.