Abstract

Low-energy hydrogen ion bombardment is used to clean GaAs surfaces. The hydrogen ions produce contamination-free surfaces without changes in surface composition (stoichiometry) and surface roughness. The wafers were brought into contact at room temperature after cleaning under ultra-high vacuum (UHV), and bonded over the whole area (2 inches) without application of external mechanical pressure. After bonding, the p-GaAs/n-GaAs wafer pair was annealed at 200 °C for 30 min under UHV conditions (<5×10 −10 mbar) to improve the interface bonding strength and to achieve a full-area wafer bonding. Infrared (IR) imaging of the as-bonded wafers directly reveal the real bonding behaviour. High-resolution transmission electron microscopy images reveal that the wafers have been directly bonded without damage of the crystal lattice or intermediate layer and the interface is smooth. Current–voltage characterization shows near-ideal forward characteristics and the recombination in p–n junction space charge region.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.