Abstract

Tungsten heavy alloy (WHA) is an ideal material employed for kinetic energy penetrators due to its high density and excellent mechanical properties. However, it is difficult to obtain ultrafine-grained tungsten alloy with excellent properties by traditional powder metallurgy method because of severe grain growth at a high sintering temperature with a long soaking time. In this study, the sintering behavior of tungsten alloys was studied at 800 to 1300 °C, and highly dense 93W-5.6Ni-1.4Fe (wt.%) WHA was successfully fabricated at a low temperature of 950 °C with a high pressure of 150 MPa by spark plasma sintering. The as-sintered tungsten alloy possesses a high relative density (98.6%), ultrafine grain size (271 nm) and high dislocation density (2.6 × 1016 m−2), which results in excellent properties such as a high hardness (1079 HV1). The high sintering pressure is considered to support an additional driving force for the sintering and lead to a low-temperature densification, which effectively limits grain growth.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call