Abstract

The internal modification of glass using ultrashort pulse lasers has been attracting attention in a wide range of applications. However, the remarkably low processing speed has impeded its use in the industry. In this study, we achieved ultrafast internal modification of glass by coaxially focusing a single-pulse femtosecond laser and continuous-wave (CW) laser with the wavelength that is transparent to the glass. Compared with the conventional method, the processing speed increased by a factor of 500. The observation of high-speed phenomena revealed that the CW laser was absorbed by the seed electrons that were generated by the femtosecond laser pulse. This technique may help expand the applications of femtosecond lasers in the industry.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.