AbstractFilms of pure and high‐impact atactic polystyrene were prepared by the recently developed technique of solid‐state coextrusion. The films were produced at extrusion rates ≥4 cm/min at 126°C with a maximum extrusion draw ratio (EDR) of 11.6. These ultradrawn films are fibrous, have a high birefringence of −2.24 × 10−2, and exhibit a 72% elastic recovery. The material has a tensile modulus of ∼4–5 GPa and a tensile strength to break of 85 MPa. Thermal analysis suggests a constant Tg.