There are several millions of weld joints made at ecorner of the world. There are chances that sa fety may be ceased to exist because of some defects in the weld joints. The obj ective of this investigation was to verify the influence of current and voltage on porosity found inside weld joints and other visual defects. Non - Destructive testing was carried out for standard butt joint from Manual metal arc welding (stick welding) and Gas me tal arc welding. Porosity was measured in terms of depth from the surface of weld joint. The results will be presented in this paper with interesting finding with test sample by different welding technique.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: International Journal of Research in Engineering and Technology
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.