Herein, a new sepiolite/alumina aerogel composite with outstanding toughness and machinability was prepared using AlCl3·6H2O precursor and sepiolite fibers by a specific sol–gel process and supercritical fluid drying. Sepiolite was added into the aluminum sols containing as high as 37 wt% of AlCl3·6H2O and the resulting sepiolite fibers dispersed randomly and uniformly with the lengths of 60–100 nm and diameters of 2–3 nm. With the increase in the ratio of sepiolite, the sepiolite-alumina aerogel composites exhibit no shrinkage during the sol–gel process and supercritical fluid drying, while a linear shrinkage of 4.6% was observed after heat-treatment at 1000 °C. Compared with undoped alumina aerogels, the sepiolite/alumina aerogel composites exhibit outstanding toughness and machinability on grinding, slicing and perforating. Meanwhile, the morphology, phase nature, and porosity of sepiolite/alumina aerogel composites with different sepiolite content (from 0 to 0.06 g/cm3) were investigated.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.