Two component silicone modified epoxy resin based low surface energy and non-toxic foul release coatings were developed. Silicone modified epoxy resin with 15 and 30% silicone content was used as component A and a polyether diamine (Jeffamine-500) was used as the component B. Free standing films were prepared by casting a mixture of components A and B in stoichiometric proportions. The surface composition, surface topography and wetting properties of the coatings were studied by angle resolved X-ray photoelectron spectroscopy (XPS), atomic force microscopy (AFM) and contact angle goniometry respectively. The mechanical properties of the cured films were evaluated by tensile measurements as well as dynamic mechanical analysis. Pseudobarnacles made of aluminium studs were attached to the coated panels and adhesion tests were carried out by a pseudobarnacle tester. Coated panels were exposed in Mumbai harbor for fouling studies for a period of 90 days. Surface restructuring studies of the coatings upon immersion in seawater were carried out by measuring the changes in advancing and receding contact angles by contact angle goniometry. The effect of surface energy, modulus and surface restructuring of the coatings on the macrofouling and pseudobarnacle adhesion properties has been discussed in detail.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.