ABSTRACTIn order to improve the adhesion strength of acrylic adhesive to untreated poly(ethylene terephthalate) (PET) substrate, two‐component acrylic structural adhesives initiated by tributylborane were prepared. The effects of acrylic monomers, elastomers, decomplexers, and oligomers on the adhesion properties of two‐component acrylic structural adhesive were investigated in sequence. It is found that the shear strength on PET of adhesives toughened by acrylonitrile–butadiene–styrene copolymer and carboxyl‐terminated butadiene–acrylonitrile copolymer is higher than that of commercial adhesives Dp8010NS and Loctite 3030. A tailored oligomer was synthesized from hydroxyl propyl–terminated polydimethylsiloxane and 3‐isopropenyl‐α,α‐dimethylbenzyl isocyanate. It is also noticed that premature failure usually takes place in the lap shear test samples due to the brittleness of the acrylic adhesive, except in the sample of adhesive modified by tailored oligomer. Excellent adhesion to the PET substrate is achieved by this adhesive modified by tailored oligomer, with a lap shear strength above 11 MPa and T‐peel strength up to 5.34 N/mm. Additionally, the resulting adhesive is qualified for the structural bonding of PET materials. © 2018 Wiley Periodicals, Inc. J. Appl. Polym. Sci.2018,135, 46612.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.