A selection of pyrene-based liquid crystal dimers have been prepared, containing either methylene-ether or diether linked spacers of varying length and parity. All the diether linked materials, CBOnO.Py (n=5, 6, 11, 12), exhibit conventional nematic and smectic A phases, with the exception of CBO11O.Py which is exclusively nematic. The methylene-ether linked dimer, CBnO.Py, with an even-membered spacer (n=5) was solely nematogenic, but odd-members (n=6, 8, 10) exhibited both nematic and twist-bend nematic phases. Replacement of the cyanobiphenyl fragment by cyanoterphenyl giving CT6O.Py, gave elevated melting and nematic-isotropic transition temperatures, and SmA and SmCA phases were observed on cooling the nematic phase. Intermolecular face-to-face associations of the pyrene moieties drive glass formation, and all these materials have a glass transition temperature at or above room temperature. The stability of the glassy twist-bend nematic phase allowed for its study using AFM, and the helical pitch length, PTB , was measured as 6.3 and 6.7 nm for CB6O.Py and CB8O.Py, respectively. These values are comparable to the shortest pitch of a twist-bend nematic phase measured to date.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.