AbstractTurning and drilling tests have been carried out on nine different materials.The most critical factor in turning is the breakouts at the corners of the test-specimen, especially at low densities. These can be eliminated by adopting a lower feed and smaller depth of cut. The best surface finish is achieved with the highest possible speed and low cut depth. Alloying iron with 0·5% sulphur resulted in the lowest recorded specific cutting force, a good surface finish, and the longest tool life attained. The density had no influence on the tool wear.Tool life in drilling can be improved considerably by using: (a) a 40° helix angle for soft power-metallurgy materials; (b) extra-short drills. Burrs can be eliminated by shortening the chisel edge or increasing the point angle to 185°. The use of sulphur-alloyed iron resulted in a tool life many times higher than that for plain iron of the same density.Machining recommendations are given for turning and drilling the various materials.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.