Abstract

The tritium release behavior from Li 2O sintered pellets (81–88% T.D.) is examined by isothermal heating tests. (1) For the 88% T.D. specimens, the fraction of residual tritium is found to follow the square-root law of the annealing time. The rate-determining process is the migration in the connected micro-pore. (2) For the 81% T.D. specimens, which are annealed after irradiation at 630 K for 4 h, the fraction of residual tritium is also found to follow the square-root law of the annealing time. The rate-determining process is the migration in the connected micro-pore. (3) For the 81% T.D. specimens as irradiated, the tritium release rate is found to follow the square-root law of the annealing time. The rate-determining process is controlled by Kohlrauch stretched exponential form. Tritium trapped in irradiation defects released with recovering the defects by isothermal heating.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.