Abstract

In the work are studied the differential parameters of wear and wear resistance of high-tech composite coatings of powder superalloys with nickel matrix, WC-12Co and mixed compositions. Coatings were created and applied to a substrate of steel with a different flame velocity - 700 m/s and 1000 m/s without preheating the substrate and with preheating the substrate to 650° C. The wear is carried out with a "thumb-disk" tribotester under dry surface friction with fixed black corundum abrasive particles. Comparative results were obtained for the microstructure and texture of the pre- and post- friction coating, the porosity, roughness, hardness, the dependence of mass wear, the speed and wear intensity and the wear resistance of the coatings on the number of friction cycles. Influence of the flame rate and substrate temperature on wear resistance and differential wear parameters has been determined.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.