Abstract

Ti-6Al-4V alloy was laser textured with cross groove patterns and then coated with graphene or MoS2, evaluating its tribological behaviour. The samples were textured by a solid state Nd:Vanadate (Nd:YVO4) laser, making crossed grooves with two different crossing angles, 45°and 60°, shaping a rhombus-like pattern. The percentage of surface area textured was 18, 40 and 64%. Solid lubricants were deposited by the cloth burnishing technique. Bidirectional sliding wear tests were performed to evaluate the tribological behaviour of the alloy. Lubricant working lifetimes were longer on textured and coated surfaces than on polished surfaces. Graphene presented longer lifetime than the MoS2 for 18 and 40% of textured density but rather similar for the 64%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.