Abstract

Targeting higher toughness transparent ceramics, tetragonal (3 mol % yttria) and cubic (8 mol % yttria) ZrO2 starting powder mixtures were densified by spark plasma sintering (SPS) in vacuum at 1100 °C and post hot isostatic pressing (HIP) in argon at 1100 °C. The influence of the ultra-fine microstructure and phase composition on the fracture resistance and light transmission in the visible and infra-red range was assessed. Of special interest was the influence of a thermal annealing step in air on the transparency of the SPS and SPS-HIP ceramics.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.