Abstract

Lead lanthanum zirconate titanate (PLZT9/65/35) ceramics were prepared from their oxide mixture via reactive sintering without involving a calcination step. PLZT ceramics sintered at 1000 °C for 4 h possessed a grain size of 3–4 μm, a dielectric constant of 3670, a dielectric loss of 0.033 at 1 kHz, and a remnant polarization of 5.7 μC/cm2 and coercive field of 4.6 kV/cm, respectively. Transparent PLZT ceramics were obtained by annealing the sintered samples at 1125 °C for 6 h repeatedly for 4 times without using hot pressing or oxygen flow. The grain size of PLZT ceramics increased to 4–6 μm, with dielectric constant of 5187 and dielectric loss (1 kHz) of 0.036, and remnant polarization of 11 μC/cm2 and coercive field of 5.3 kV/cm. The transparent PLZT ceramics demonstrated a transmittance of 42% at a wavelength of 550 nm.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.