Abstract
We present a simple model to explain the transition from oscillatory to smooth crack propagation in brittle metallic glasses. We demonstrate that the smooth fracture propagation that is characteristic for higher temperature or higher crack opening velocities (for type 1 crack propagation) becomes unstable and oscillatory behavior is being observed. The characteristic feature size of the crack propagation may be at the nanometer scale and grows as the opening velocity decreases.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.