In continuous slab casting at OAO Magnitogorskii Metallurgicheskii Kombinat (MMK), metal of different grades in a series is separated by leaving an appropriate quantity of steel from the previous melt in the intermediate ladle. The losses of metal are least on leaving around 12 t of steel in the intermediate ladle. The mass of the transition sections of mixed composition in the bar billet is 2.5 times the mass of the steel left in the ladle.