Abstract

Three kinds of tungsten coatings are fabricated by means of APS and CVD, and evaluated by transient high heat load tests by 25 high-intensity current pulsed electron beam pulses with a duration of 0.2ms and power densities of 0.4, 0.6 and 0.8GW/m2. Remelting and solidification are found on post-test APS-W coating. However, cracks are developed for the same power densities for the CVD-W coating. APS-W coatings have about 20 times mass loss of CVD-W coating. The mass loss is related to the peak surface temperature of the APS-W coating exceeding the tungsten melting point (3410°C) during electron beam irradiation. The CVD-W coating during testing was only 1000°C.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.