Abstract

ABSTRACTMeasurements were made of the conductance of single crystal Au-doped Si and silicon-on-sapphire (SOS) during irradiation with 30 nsec ruby laser pulses. After the decay of the photoconductive response, the sample conductance is determined primarily by the thickness and conductivity of the molten layer. For the single crystal Au-doped Si, the solid-liquid interface velocity during recrystallization was determined from the current transient to be 2.5 m/sec for energy densities between 1.9 and 2.6 J/cm2, in close agreement with numerical simulations based on a thermal model of heat flow. SOS samples showed a strongly reduced photoconductive response, allowing the melt front to be observed also. For complete melting of a 0.4 μm Si layer, the regrowth velocity was 2.4 m/sec.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.