Abstract

The effect of the thickness of the amorphous polymerized films of poly-4,4'-diphenylene oxide pyromellitimide on the structure after deformation by stretching at 293 K and 77 K was studied. The evolution of the macromolecular structure was concluded based on the results of the redistribution of the intensity diffraction peaks. It was established that the structure of films with a thickness of 75 μm is homogeneous and does not cardinal changes after deformation. Deformation of polymer films with a thickness of 125 μm leads to the appearance of regions with long-range order in the sample.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.