The transformation of pentlandite, (Ni,Fe) 9 S 8 , to violarite, (Ni,Fe) 3 S 4 , has been investigated under mild hydrothermal conditions, at constant values of pH (range 3 to 5) controlled by the acetic acid/sodium acetate buffer. At 80 °C, 20(4) wt% of the pentlandite transforms to violarite in 33 days; with the addition of small amounts of Fe 3+ (CH 3 COO) 2 (OH) and H 2 S the reaction reaches 40(4) wt% completion in this time. At 120 °C and a pressure of 3.5 bars the reaction is complete in 3 days at pH 3.9. Electron backscatter diffraction and backscattered electron imaging reveal that the reaction textures are typical of a coupled dissolution-reprecipitation reaction, rather than a solid state electrolytic process as has been previously reported. The gap between the dissolution front and the precipitation front of violarite is less than 400 nm. The violarite produced by these hydrothermal transformations is texturally similar to supergene violarite, being fine grained, porous and finely cracked.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.