Abstract

Transformations of Pt/TiO2 catalyst between non-SMSI and SMSI states have been investigated by repeatedH2−O2 titration. The decline of capacity of H2 and O2 chemisorption and their reaction on Pt particles is accountable by reduction of superficial labile oxygen species in the temperature range of 298–573 K and an increase of surface oxygen vacancies on TiO2 above 573 K, respectively.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.