Abstract

In Ni–Cu alloys, iron must be excluded in many cases. Iron may enter the alloy from the batch or the furnace lining. Since the Fe2O3 content in refractories may be as much as 2.5%, it is important to assess the increase in iron content in alloys on account of interaction with the furnace lining. In the present work, the influence of the Fe2O3 content in the crucible and the volume of the crucible on the iron content in the final alloy is studied. Thermodynamic analysis and experimental data indicate that the nickel and copper in Ni–Cu alloys may reduce iron that is present in the lining. When using low-iron batch, iron from the crucible is transferred almost completely to the melt. The increase in iron content in Ni–Cu alloys is investigated as a function of the capacity of the vacuum induction furnace and the Fe2O3 content in the periclase crucibles, with complete transfer of the iron from the lining to the melt. With increase in furnace capacity, less iron enters the melt from the crucible. With more than 200 kg of metal, the increase in iron concentration mainly depends not on the furnace capacity but on the Fe2O3 content in the refractory. In order to produce Ni–Cu alloys with <0.01% Fe, refractories with Fe2O3 content no higher than 0.5% must be used. To produce Ni‒Cu alloys with <0.05% Fe, the use of lining refractories with Fe2O3 content no higher than 2.5% is recommended.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.