By means of the radioactive-tracer sectioning technique, the tracer diffusion of the impurity ions, 46Sc, 51Cr, 54Mn, 59Fe, 60Co, 63Ni and 95Zr, in rutile single crystals was measured as functions of crystal orientation, temperature, oxygen partial pressure and Al impurity content. The diffusion coefficients are very sensitive to the electric charge of the impurity ions. Divalent impurities (e.g., Co and Ni) diffuse extremely rapidly in TiO 2, compared to cation self-diffusion, and exhibit an extreme anisotropy in diffusion behavior, divalent-impurity diffusion parallel to the c-axis is much larger than it is perpendicular to the c-axis. Trivalent impurity ions (Sc and Cr) and tetravalent impurity ions (Zr) diffuse similar to cation self-diffusion, both as functions of temperature and oxygen partial pressure. The divalent impurity ions Co and Ni apparently diffuse as interstitial ions along open channels parallel to the c-axis. The results suggest that Sc, Cr and Zr ions diffuse by an interstitialcy mechanism involving the simultaneous and cooperative migration of tetravalent interstitial titanium ions and the tracer-impurity ions. Iron ions diffuse both as divalent and as trivalent ions. The impurity diffusion as functions of oxygen partial pressure and Al-impurity content are consistent with calculations of point-defect concentrations in rutile.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.