Abstract

ABSTRACTThe deposition of TiO2-P25 on Pyrex glass is studied in order to propose a procedure for obtaining uniform and adherent thin films with a controlled thickness in the range between fractions of micrometer to a few tens of micrometers. Different deposition methods such as spray-coating, dip-coating, and drop-coating of liquid suspensions of TiO2-P25 powder are considered. The effects of pretreatment of the glass support, as well as postdeposition steps such as drying condition and thermal treatment, are also reported. A basic glass pretreatment and an acidic TiO2 suspension are chosen for an optimized adherence of the film. Drop-coating, associated with a slow drying under 55% relative humidity and a high-temperature thermal treatment is the method of choice to prepare coated glass slides in a large range of film thicknesses.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.