The effect of addition of organoclay and the reactive ABS‐g‐MA core‐shell particles on the mechanical properties and morphology of blends of polyamide (PA6) were reported. The reactive rubber particles with core‐shell structure were selected as modifier instead of conventional reactive bulk rubber. The microstructure of the ternary nanocomposites was characterized by X‐ray diffraction (XRD), transmission electron microscopy (TEM), and scanning electron microscopy (SEM). Impact strength and stress–strain behavior of blends were measured as a function of organoclay content and core/shell ratio of ABS‐g‐MA. The organoclay plates affected the interfacial adhesion between polyamide and the core‐shell particles because of a shielding effect of organclay on the interacting of amine end groups of PA6 with the MA groups of ABS‐g‐MA. The poor dispersion behavior of ternary nanocomposites was observed when the core/shell ratio is 80/20, and with an increase of organoclay content, the core/shell dispersed phase size increased. Blends based on the maleated elastomer with the core/shell ratio 60/40 gave a more beneficial balance of toughness versus stiffness. POLYM. COMPOS., 35:864–871, 2014. © 2013 Society of Plastics Engineers

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.