Abstract

Molybdenum disilicide (MoSi2) with or without La2O3 particles were synthesized by mechanical alloying (MA) and HP techniques. The fracture toughness at room temperature was measured by Anstis’ mode and the responded microstructures were analyzed by using SEM and X-ray. The results show that the addition of La2O3 could obviously toughen the matrix. When the content of La2O3 in MoSi2 is about 0.9%, the fracture toughness value increases by about 50% more than that of pure MoSi2. We think, the corresponding toughening mechanisms depend on the following: fine-grain, microcracking, crack deflection, crack microbridging, crack bowing and branching.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.