Abstract

The development of hot‐pressed Sic‐whisker‐reinforced alumina has resulted in composites with fracture toughness values ∼;8.7 MPa·m112 at 20 vol% SiC. Whisker orientation during processing leads to anisotropy in both fracture toughness and fracture strength. Fracture strengths are also limited by the ability to disperse the Sic whiskers; however, use of both fine alumina powders and ultrasonic dispersion techniques yields strengths ∼;800 MPa.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.