Abstract

The torsional properties of stainless steel (SS) endodontic files (Flex-O-File; Maillefer/L. D. Caulk Co., Milford, DE) and recently developed nickel-titanium (NiTi) endodontic files (Quality Dental Products, Inc., Johnson City, TN) were compared. File sizes 15, 25, 35, 45, and 55 were subjected to torsional load in clockwise (CW) and counterclockwise (CCW) directions independently. Results showed that SS files had a significantly greater rotation to failure in the CW direction, whereas the NiTi files had a significantly greater rotation to failure in the CCW direction. Despite these differences in rotation to fracture, there was essentially no difference between the SS and NiTi instruments in the torque that it took to cause failure in both the CW and the CCW directions. Therefore, whereas the number of CW and CCW rotations to failure differed for the two instruments, the actual force that it took to cause that failure was the same.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.