Corncob was torrefied under nitrogen and carbon dioxide atmospheres at 220–300 °C, obtaining solid products with mass yields of 69.38–95.03% and 67.20–94.99% and higher heating values of 16.58–24.77 MJ/kg and 16.68–24.10 MJ/kg, respectively. The changes of physicochemical properties of the charcoal was evaluated by many spectroscopies, contact angle determination, and combustion test. Hemicelluloses were not detected for the torrefaction under the hard conditions. As the severity increased, C concentration raised while H and O concentrations reduced. Combustion test showed that the burnout temperature of charcoal declined with the elevation of reaction temperature, and torrefaction at a high temperature shortened the time for the whole combustion process. Base on the data, torrefaction at 260 °C under carbon dioxide was recommended for the torrefaction of corncob.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.