AbstractSmooth titanium silicide films have been deposited using a Low Pressure Chemical Vapor Deposition (LPCVD) process. A system has been designed and built for the LPCVD of titanium silicide. It is a cold wall reactor with the wafer being heated externally by infrared lamps. Sequential deposition of polycrystalline silicon (polysilicon) and titanium silicide films, and in-situ annealing of these films, if required, can be performed in this system. A turbomolecular pump is used to provide a contaminant free environment with a base pressure of <10−7 torr. SiH4 and TiCl4 are used as silicon and titanium sources, respectively.Tithnium silicide films with resistivities ranging from 22 to 39 μΩ-cm have been obtained. At low deposition rates, these films have surface roughnesses ranging from 50 to 250 Å. From X-ray diffractometry, it was determined that the as-deposited titanium silicide films were polycrystalline, and TiSi2 was the predominant phase. Si/Ti ratios of 1.8 to 2.3 were obtained frog Rutherford Backscattering Spectroscopy (RBS). Auger analyses did not show any impurities such as oxygen, carbon or chlorine in these films.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.