Abstract
Titanium oxide thin film, fabricated with tetraisopropyltitanate and oxygen by electron cyclotron resonance-plasma-enhanced chemical vapor deposition, is investigated as a potential candidate for the antireflective layer in KrF excimer laser (248-nm) lithography. The oxygen flow-rate dependence of the optical properties such as the refractive index (n) and the extinction coefficient (k) of the film at the 248-nm wavelength has been characterized, and the films with the expected combinations of n and k values for the antireflective layer have been deposited. Simulation results indicate that reflectance values of less than 4% and as low as 1.2% can be reached at the interface between the photoresist and the film postulating the structures of the photoresist/300-A TiO(x) film/c-Si substrate and the W-Si substrate, respectively, by selected proper combinations of n and k values. Moreover the reflectance can be further reduced to almost zero by changing the film thickness. Thus it is found that titanium oxide thin films can be used as the bottom antireflective layer in KrF excimer laser lithography.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.