Abstract
A harmonic-structured composite with a fine grain Ti-48 mol%Al alloy network and dispersed coarse grain pure titanium is produced by extrusion sintering using the spark plasma sintering (SPS) process. The conditions of extrusion sintering by the SPS process are a sintering temperature of 1073 K, a holding time of 1.8 ks and an extrusion pressure of 100 MPa with a pressurization rate of approximately 0.1 MPa/s. The extrusion compact has a rod shape with φ5×48 mm. The extrusion compact is composed of an elongated harmonic structure with the Ti-48 mol%Al alloy network and the dispersed pure titanium. The Vickers hardness of the extrusion compact is about 220 Hv, which is almost the same as that of a conventional compact.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of the Japan Institute of Metals and Materials
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.