We synthesized Ti oxide nano-porous structure on the surface of Ti–Cu amorphous alloy in a HNO 3 solution using a dealloying method. The influences of HNO 3 concentration, reaction temperature and load voltage on the morphology of the nano-porous structure were investigated. The mean diameter of nano pores was about 50 nm and the thickness of pore walls is about 100 nm. The nano-porous surface was composed of Ti and Cu oxides.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.