We previously proposed a new method to synthesize nano-sized powders of various alloys and intermetallic compounds. The method consisted of electrical wire explosion of electrodeposted metal wires. In this study, the method was applied for Ti-Cr alloy. The overall composition of the Cr-coated Ti wire was about Ti-25 at% Cr. The explosion products consisted of equilibrium phases of α-Ti and TiCr2 phases along with meta-stable Ti-rich β phase. The composition of β phase estimated from its lattice parameter was Ti-13 at% Cr. The β phase decomposed completely to α-Ti and TiCr2 phases during isothermal aging at 600°C for one day.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.