Luminescence spectra, power dependence and luminescence lifetimes were measured and studied in pure cubic phase NaYF4:20%Yb3+, x%Tm3+ (where x=0.1%, 0.2%, 0.5%, 1% and 2%) nanocolloidal phosphors synthesized by thermal decomposition. Increasing concentration of Tm3+ ions led to decrease of luminescence intensity, increase in the slopes of power dependence as well as to the decrease in the luminescence decay- and rise-times, helping to resolve the mechanisms of up-conversion and concentration quenching.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.