Lasing action at 1.73, 1.23, and 0.85 μm was obtained by a threefold upconversion process in Er:YLF at 110 K using a 1.53 μm Er:glass pump laser. The 1.73 μm transition had the lowest threshold and highest pump conversion efficiency.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.