Abstract

Susceptibility artifacts generated in magnetic resonance (MR) images were quantitatively evaluated for various metals using a three-dimensional (3-D) artifact rendering to demonstrate the correlation between magnetic susceptibility and artifact volume. Ten metals (stainless steel, Co–Cr alloy, Nb, Ti, Zr, Mo, Al, Sn, Cu and Ag) were prepared, and their magnetic susceptibilities measured using a magnetic balance. Each metal was embedded in a Ni-doped agarose gel phantom and the MR images of the metal-containing phantoms were taken using 1.5 and 3.0T MR scanners under both fast spin echo and gradient echo conditions. 3-D renderings of the artifacts were constructed from the images and the artifact volumes were calculated for each metal. The artifact volumes of metals decreased with decreasing magnetic susceptibility, with the exception of Ag. Although Sn possesses the lowest absolute magnetic susceptibility (1.8×10−6), the artifact volume from Cu (−7.8×10−6) was smaller than that of Sn. This is because the magnetic susceptibility of Cu was close to that of the agarose gel phantom (−7.3×10−6). Since the difference in magnetic susceptibility between the agarose and Sn is close to that between the agarose and Ag (−17.5×10−6), their artifact volumes were almost the same, although they formed artifacts that were reversed in all three dimensions.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.