Abstract

Room-temperature sodium-sulfur (RT Na-S) battery cathodes suffer from poor conductivity, rapid dissolution of intermediate products, and potentially destructive volume change during cycling. The optimal way to minimize these problems could be a construction of a nanocomposite cathode scaffold combining different components selected for their particular functions. Here, we have combined the excellent electronic conductivity of reduced graphene oxide, polysulfide adsorption ability of the ultrafine manganese oxide nanocrystals, rapid ion/electron dissemination efficiency of nanosized sulfur, and outstanding mechanical stiffness and good electrical conductivity of Na alginate/polyaniline hybrid binder in a single electrode heterostructure. At 0.2 A g-1, an RT Na-S battery containing the freestanding cathode delivers an initial specific cap acity of 631 mA h g-1. By delivering a nominal discharge voltage of 1.81 V, our Na-S batteries bestow a high specific energy of 737 W h kg-1 at the 2nd cycle and 660 W h kg-1 was retained after 50 cycles. The effect of the amount of electrolyte additive is also well demonstrated in this study. The electrode fabrication process provides a new approach to tailor the design and preparation of effective cathodes for the room-temperature sodium-sulfur batteries.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.