Abstract

A high resolution three-dimensional scanning technique called X-ray microtomography was used to measure internal crack growth in small mortar cylinders loaded in uniaxial compression. Tomographic scans were made at different load increments in the same specimen. Three-dimensional image analysis was used to measure internal crack growth during each load increment. Load–deformation curves were used to measure the corresponding work of the external load on the specimen. Fracture energy was calculated using a linear elastic fracture mechanics approach, but using the actual surface area of internal cracks created. Preliminary results indicate fracture energies in the same range as those measured using traditional techniques.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.