Abstract
All coefficients of the third-column of the unclamped and clamped electro-optic tensor of zirconium-doped congruent LiNbO3 single crystals, in the concentration range up to 2.5mol%, are determined as function of the dopant concentration by direct techniques based on interferometric and Sénarmont optical arrangements at the wavelength of 633nm and at room temperature. It is found that all the unclamped and clamped electro-optic coefficients are relatively constant, except for the sample doped with 2mol% of zirconium. From the obtained experimental values, the acoustic contribution is then deduced and found constant over all the studied samples. Finally, the electro-optic behavior of LN:Zr as function of the dopant concentration was confirmed by dielectric characterizations.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.