While extensive research on the lead-free solder has been conducted, the high melting temperature of the lead-free solder has detrimental effects on the packages. Thermosonic bonding between metal bumps and lead-free solder using the longitudinal ultrasonic is investigated through numerical analysis and experiments for low-temperature soldering. The results of numerical calculation and measured viscoelastic properties show that a substantial amount of heat is generated in the solder bump due to viscoelastic heating. When the Au bump is thermosonically bonded to the lead-free solder bump (Sn-3%Ag-0.5%Cu), the entire Au bump is dissolved rapidly into the solder within 1 sec, which is caused by the scrubbing action of the ultrasonic. More reliable solder joints are obtained using the Cu/Ni/Au bump, which can be applied to flip-chip bonding.