Summary: Temperature-sensitive P(DEAEMA-co-DMAAm) cryogels with five different DMAAm contents were synthesized via a two-step polymerization method, the initial polymerization being conducted for various times at 22 °C, followed by polymerization at −26 °C for 24 h. The influence of the first-step time and the content of DMAAm on the swelling ratio and network parameters such as the polymer/solvent interaction parameter, the average molecular mass between crosslinks, and the mesh size of the cryogels were reported and discussed. The swelling studies indicated that the swelling increased in the following order: 22C45 > 22C30 > 22C15 > 22C0. The cryogels exhibited swelling/deswelling transitions (reentrant phenomena) in water depending on temperature. These properties were attributed to the macroporous and regularly arranged network of the cryogels. Scanning electron microscope graphs reveal that the macroporous network structure of the cryogels can be adjusted by applying a two-step polymerization. Chemical structure of the P(DEAEMA-co-DMAAm) cryogels.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.