Composites of thermoplastic starch (TPS) with titanium dioxide particles (mTiO2; average size 0.1μm) with very homogeneous matrix and well-dispersed filler were prepared by a two-step method, including solution casting (SC) followed by melt mixing (MM). Light and scanning electron microscopy confirmed that only the two-step procedure (SC+MM) resulted in ideally homogeneous TPS/mTiO2 systems. The composites prepared by single-step MM contained non-plasticized starch granules and the composites prepared by single-step SC suffered from mTiO2 agglomeration. Dynamic mechanical measurements showed an increase modulus with increasing filler concentration. In TPS containing 3wt.% of mTiO2 the stiffness was enhanced by >40%. Further experiments revealed that the recommended addition of chitosan or the exchange of mTiO2 for anisometric titanate nanotubes with high aspect ratio did not improve the properties of the composites.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.